Moabfighter
Well-Known Member
With the pretty holes and stuff in it? A vacuum or something? How much are they. Can anyone steer me to an inexpensive way to turn my butane into trim goolash into shatter? Thanks.
The stuff with the holes is an early pour, usually on parchment or PTFE film. It's placed in a preheated vacuum oven or chamber around 85/115F and purged under around 10,000 microns/29.5" Hg vacuum.With the pretty holes and stuff in it? A vacuum or something? How much are they. Can anyone steer me to an inexpensive way to turn my butane into trim goolash into shatter? Thanks.
What do you mean by, "an early pour"?The stuff with the holes is an early pour, usually on parchment or PTFE film. It's placed in a preheated vacuum oven or chamber around 85/115F and purged under around 10,000 microns/29.5" Hg vacuum.
It means that it is poured or discharged from the closed loop extraction system early and the balance of the purge done on parchment or film in a heated vacuum chamber or oven. It typically has more and larger gas bubbles than open blast finished the same way.What do you mean by, "an early pour"?